Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0103 GPa | 1.50 ksi | ASTM D790 |
Lubrizol Estane® ALR PC85A Thermoplastic Polyurethane Type: Estane® ALR PC85A is a polycarbonate diol based thermoplastic polyurethane (TPU).Features: Hydrolytically stable, very durableAvailable in Americas, Europe, Middle East, Africa, India and Asi.. |