Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.345 GPa | 195.1 ksi | ASTM D790 |
Eastman Tenite 360E0096914 Cellulose Acetate Propionate, Natural, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Flexural Modulus | 1.345 GPa | 195.1 ksi | ASTM D790 |
Eastman Tenite 360E4861314 Cellulose Acetate Propionate, Clear, Trsp Applications:ProfilesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. T.. |
|||
Flexural Modulus | 1.345 GPa | 195.1 ksi | ASTM D790 |
Chevron Phillips Marlex® HXB TR-512 Extra high molecular weight polyethylene Benefits: outstanding impact and creep resistance, excellent ESCR, excellent chemical resistanceCharacteristics: ESCR > 700 at Condition A, at 50°C; ASTM D 1693Applications: 55-gallon drums, indust.. |
|||
Flexural Modulus | 1.345 GPa | 195.1 ksi | ASTM D790 |
ALM D80-ST Nylon 11 SLS Prototyping Polymer Unfilled, color stabilized nylon 11 material that is also stabilized to prevent premature thermal degradation. Parts produced from PA D80-ST exhibit superior mechanical properties. Relatively inexp.. |
|||
Flexural Modulus | 1.345 GPa | 195.1 ksi | ASTM D790 |
ALM FR 106 Nylon 11 SLS Prototyping Polymer This flame retardant rapid prototyping material has additives in the raw material that allows it to pass aeronautic standard FAR25.853 smoke, flame, and toxicity tests. This material is ideal for Ae.. |