Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 1.034 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.034 GPa
150.0 ksi
ISO METHOD 178
NYCOA 2061 Copolymer Nylon 6/69
monofilament weed eater, fishing lineInformation provided by NYCOA, Inc.
Flexural Modulus 1.034 GPa
150.0 ksi
ASTM D790
Chevron Phillips Marlex® HMN 4550 High Density Polyethylene  (discontinued **)
High Density PolyethyleneCustomer Benefits: This resin is a high density polyethylene copolymer with high stress crack resistance, outstanding impact strength, and good warpage resistance. It is us..
Flexural Modulus 1.034 GPa
150.0 ksi
2% Secant; ASTM D790
Ineos HP55-25-155 HDPE
A high performance high density polyethylene copolymer developed for blow molding. It is recommended for use in continuous extrusion blowmolding equipment, specifically where applications require ex..
Flexural Modulus 1.034 GPa
150.0 ksi
ASTM D790
Lucent Polymers TPP-310 Polypropylene, 10% Talc Filled, Impact Modified
Melt Flow Adjustable for ApplicationAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 1.034 GPa
150.0 ksi
ASTM D790
Lucent Polymers PPC-210 Polypropylene, Impact Modified
Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 1.034 GPa
150.0 ksi
ASTM D790
Lucent Polymers PPC-220 Polypropylene, Impact Modified
Add "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 1.034 GPa
150.0 ksi
ASTM D790
Eastman Tenite 285A2R30018 Cellulose Acetate Butyrate, Natural, Trsp
Applications:OphthalmicsOptical safety framesProduct Description: Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, cla..
Flexural Modulus 1.034 GPa
150.0 ksi
ASTM D790
Eastman Tenite 285A3R30018 Butyrate Natural, Trsp
Tenite cellulosic plastics are noted for their excellent balance of properties - toughness, hardness, strength, surface gloss, clarity, and a warm feel. The mechanical properties of Tenite cellulosi..
Flexural Modulus 1.034 GPa
150.0 ksi
CMW® ELKONITE® 2188 Infiltrated Tungsten Silver Contact Material
High wear resistance and reliability.Information provided by CMW Inc.
Flexural Modulus 1.034 - 1.241 GPa
150.0 - 180.0 ksi
ASTM D790
Arkema Group KYNAR FLEX® 2850 Black Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating, pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Flexural Modulus 1.034 - 1.241 GPa
150.0 - 180.0 ksi
ASTM D790
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Flexural Modulus 1.034 - 1.241 GPa
150.0 - 180.0 ksi
ASTM D790
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Flexural Modulus 1.034 GPa
150.0 ksi
1% Secant; ASTM D790
Ravago Manufacturing Americas Echo® RPPC 20/2 BK Recycled Polypropylene
Copolymer Polypropylene, Unreinforced, 20 MFI, 2 Izod, BlackEntecs proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, ..
Flexural Modulus 1.034 GPa
150.0 ksi
ASTM D790
Lucent Polymers PPC-0222 Polypropylene, Impact Modified
Recycled ContentAdd "U" for UV StabilizedAdd "H" for Heat StabilizedInformation provided by Lucent Polymers, Inc.
Flexural Modulus 1.034 - 1.241 GPa
150.0 - 180.0 ksi
ASTM D790
Arkema Group KYNAR FLEX® 2850-00 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Flexural Modulus 1.034 - 1.241 GPa
150.0 - 180.0 ksi
ASTM D790
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani..
Copyright © lookpolymers.com All Rights Reserved