Mechanical Properties Metric English Comments
Flexural Modulus 0.981 - 9.51 GPa
142 - 1380 ksi
Average value: 3.93 GPa Grade Count:18
Overview of materials for Polyphenylene Ether, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 10% Glass Filled". Specific grades with glass content between 5% and 14% are includ..
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
Hyosung Topilene C600Y PP
C600Y Butene Random CopolymerApplications: FilmCharacteristics:Excellent transparency & glossLow sealing temperatureHigh hot-tack strengthGood stiffnessInformation provided by Hyosung Corporation
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
Hyosung Topilene R500F PP
R500F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
Hyosung Topilene R500S PP
R500S Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation
Flexural Modulus 0.981 GPa

@Thickness 3.20 mm
142 ksi

@Thickness 0.126 in
15mm/min; ASTM D790
LG Chemical LUCON PO6062 mPPO+CNT+CF+GF
Description: Injection Molding, mPPO+CNT+CF+GF, High Strength, Heat StabilityApplication: ATM parts, LCD Cell TrayCAS No. 35134-01-4, 25038-54-4, 65997-17-3, 7440-44-0 and 7782-42-5Information provi..
Flexural Modulus 0.981 GPa

@Thickness 6.40 mm
142 ksi

@Thickness 0.252 in
10mm/min; ASTM D790
LG Chemical LUPOL GP1007FE Flame Retardant PP
Description: Injection Molding, FR PP, General Purpose, Flame RetardantApplication: Electrical & Electronic, Automotive PartsCAS: 9003-07-0 and 1309-64-4Information provided by LG Chemical
Flexural Modulus 0.981 GPa
142 ksi
Olsen Stiffness; ASTM D747
Global B-8200 High Density Polyethylene
Description-high molecular weight, excellent stress cracking resistance, excellent impact strength to blow moldApplications-large drums, gasoline tanks, agricultural chemical tanksInformation provi..
Flexural Modulus 0.981 GPa
142 ksi
Olsen Stiffness; ASTM D747
Global F-7000 High Density Polyethylene
Description-high quality is suitable for blown film @wide range of size & thickness Applications-large & small rolled film, shopping bag, merchant bag, disposal waste bagInformation provided by Glob..
Flexural Modulus 0.981 GPa
142 ksi
Olsen Stiffness; ASTM D747
Global J-1600 High Density Polyethylene
Description-suitable for injection moldingApplications-household products, handy craft flowers, toys, stationaryInformation provided by Global Polymers Corporation.
Flexural Modulus 0.981 GPa
142 ksi
Olsen Stiffness; ASTM D747
Global J-2308 High Density Polyethylene
Description-industrial injection grade w/ UV stabilizer, good for high impact strengthApplications-high quality industrial products, outdoor applications such as pallets & cratesInformation provided..
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
LG Chemical LUTENE-H XL1800 HDPE
Description: LUTENE-H XL 1800 is a optimum materials for under-floor heating and drinking water pipe by RAM type extrusion. It is excellent product with long-term internal pressure creep property an..
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
LG Chemical SEETEC PB150 HDPE
Features: This high molecular weight, hexane copolymer is tailored for high impact blow-molded containers that require:Excellent processabilityHigh impact strength at low temperatureOutstanding stre..
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
Shinkong Synthetic Fibers Shinite® PP4220 PP, High Impact, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
Shinkong Synthetic Fibers Shinite® PP4210 PP, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
Shinkong Synthetic Fibers Shinite® PP4220 PP, High Impact, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Flexural Modulus >= 0.981 GPa
>= 142 ksi
ASTM D790
SCG Chemicals EL-Leneâ„¢ H2001WC High Density Polyethylene Wire & Cable Grade
Key Characteristics:Excellent environmental stress cracking resistance (ESCR), high mechanical properties, high speed extrusionRecommended Applications:Jacketing of fiber optical cablesJacketing of ..
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
SCG Chemicals EL-Leneâ„¢ H5480S High Density Polyethylene Monofilament
Key Characteristics:High tenacityExcellent product colorRecommended Applications: Monofilament and flat yarn extrusion for manufacturing of nets, ropes and tarpaulinInformation provided by SCG Chem..
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
Samyang Triel® 5720 Thermoplastics Polyetherester Elastomer, General Extrusion
Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5720 is an extrusion grade.Information provided by Samyang.
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
Shinkong Synthetic Fibers Shinite® PP4210 PP, Fire Retardant
Information from Shinkong Synthetic Fibers Corp.
Flexural Modulus 0.981 GPa
142 ksi
ASTM D790
LG Chemical LUTENE-H ME9180 HDPE
Description: LUTENE-H ME9180 is mainly intended for injection molding of complicated parts. It has high productivity and good appearance.Applications: Complicated parts, light-weight household.CAS N..