Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.740 GPa | 107 ksi | Compression Molded; ASTM D790 |
NOVA Chemicals Surpass® RMs539-U Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |
|||
Flexural Modulus | 0.740 GPa | 107 ksi | Compression Molded; ASTM D790 |
NOVA Chemicals Surpass® RMs539-UG Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |
|||
Flexural Modulus | 0.740 GPa | 107 ksi | ASTM D790 |
BASF Capron® 8200 NL Nylon 6 (Conditioned)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 0.740 GPa | 107 ksi | ASTM D790 |
BASF Capron® 8202 NL Nylon 6 (Conditioned)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Flexural Modulus | 0.740 GPa @Strain <=0.250 % |
107 ksi @Strain <=0.250 % |
ISO 178 |
Total MDPE HT 514 Medium Density Polyethylene, Blown Film MDPE HT 514 is a medium density polyethylene produced by slurry loop low pressure process with hexene as co-monomer.MDPE HT 514 is a semi-high molecular weight polyethylene giving excellent mechanic.. |
|||
Flexural Modulus | 0.740 GPa | 107 ksi | 2% Secant - 16:1 span:depth, 0.5 in/min; ASTM D-790 |
Chevron Phillips Marlex® HMN TR-945/945G Polyethylene; HDPE High density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and excellent flowLong-term UV stabilizationGood impact stren.. |
|||
Flexural Modulus | 0.740 GPa | 107 ksi | ASTM Test |
BASF Ultramid® 8202 HS PA6 (Conditioned) Ultramid 8202 HS is a heat stabilized, low viscosity, general purpose nylon 6 injection molding homopolymer. It possesses the combination of strength and toughness and has excellent chemical and ab.. |
|||
Flexural Modulus | 0.740 GPa | 107 ksi | ASTM Test |
BASF Ultramid® 8202 PA6 (Conditioned) Ultramid 8202 is a low viscosity, general purpose polyamide 6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is also available in heat stabilized (Ult.. |
|||
Flexural Modulus | 0.740 GPa @Temperature 120 °C |
107 ksi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Flexural Modulus | 0.740 GPa | 107 ksi | |
Reliance Industries Reclair Crosslinked R35042 Crosslinkable R35042 is a polyethylene grade that has increased service temperature and toughness, and improved ESCR over Reclair R35042. Crosslinkable R35042 applications include fuel tanks and ch.. |