Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 0.731 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.731 GPa
106 ksi
ASTM D790
Quadrant EPP TIVAR® 88-2 ESD Black, Premium Lubricant Filled, Lower COF, Electro Static Dissipative Lining Material (ASTM Product Data Sheet)
Flexural Modulus 0.731 GPa
106 ksi
ASTM D790
Ravago Manufacturing Americas Hylon® N2000HL Nylon 6 (Cond)
Information provided by Ravago.
Flexural Modulus 0.731 GPa
106 ksi
1% secant; ASTM D790
ExxonMobil LL 8450 Rotational Molding Resin  (discontinued **)
LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. This resin is ideally suited for applications that require optimum balance..
Flexural Modulus 0.731 GPa
106 ksi
1% secant; ASTM D790
ExxonMobil LLP8450.31 Rotational Molding Resin
LProduct Description: LL 8450 is a linear low density hexene copolymer designed to offer excellent stiffness, processability, whiteness and ESCR. They are ideally suited for applications that requir..
Flexural Modulus 0.731 GPa
106 ksi
ASTM D-790
CMT Materials REN Shape® 440 Tooling Board, Modeling Board, Adhesive Products
CMT Materials offers the complete line of REN Shape tooling board, modeling board, and related adhesive products. Vacuum formers and thermoformers use these products as prototype and low volume prod..