Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.715 GPa | 104 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXPRO® R225 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R225 is a high-impact polypropylene co-polymer molding compound. Applications: Small exterior trim components. Information provided by Solvay Engineered Polymers. LyondellBasel.. |
|||
Flexural Modulus | 0.715 GPa | 104 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXPRO® R210 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R210 is a high-impact polypropylene co-polymer molding compound. Applications: Exterior trimInformation provided by Solvay Engineered Polymers. LyondellBasell acquired Solvay E.. |
|||
Flexural Modulus | 0.715 GPa | 104 ksi | 80x10x4 mm specimen, 2 mm/min; ISO 178 |
Solvay Engineered Polymers DEXPRO® R116 TPV - High-Impact Polypropylene
(discontinued **) Description: DEXPRO® R116 is a thermoplastic polyolefin elastomeric. It is unfilled, reactor-grade molding compound. Applications: Exterior trim Information provided by Solvay Engineered Polymers.. |