Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | >= 0.550 GPa | >= 79.8 ksi | ASTM D1238 |
NIZHNEKAMSKNEFTEKHIM PE 4026Z (26460) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | >= 0.550 GPa | >= 79.8 ksi | ASTM D790 |
NIZHNEKAMSKNEFTEKHIM PE 4028X (28435) Linear Low Density Polyethylene Product obtained by gas phase polymerization of ethylene in presence of complex metalorganic catalysts.Information provided by manufacturer |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | Injection molded specimen, 0.05 in/min, Tangent method; ASTM D790 |
Phillips Sumika Marlex® ABF-080 Thermoplastic Polyolefin
(discontinued **) Applications: Air damInterior trimInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. This product had been discontinued prior t.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
3M Dyneon™ PFA X 6505 UHP Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA X 6502 UPH, PFA X 6505 UHP and PFA X 6515 UHP are ultra-high purity fluorothermoplastics. These resins were developed for high-purity applications requiring ultra-low levels of metal and .. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
3M Dyneon™ PFA 6502N Perfluoroalkoxy Fluorothermoplastic
(discontinued **) The excellent chemical temperature resistance of Dyneon™ 6500N PFA is available across a range of melt flow indices, for optimal processability. Dyneon™ PFA 6502N, the highest molecular weight gra.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
3M Dyneon™ PFA 6505N Perfluoroalkoxy Fluorothermoplastic
(discontinued **) The excellent chemical temperature resistance of Dyneon™ 6500N PFA is available across a range of melt flow indices, for optimal processability. Dyneon™ PFA 6502N, the highest molecular weight gra.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
3M Dyneon™ PFA 6502TA Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6502TA is a fluorothermoplastic resin developed for compression molding applications. PFA 6502TA has a wide processing window with excellent color stability when longer residence times or.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
3M Dyneon™ PFA 6503 A EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6503 A EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick .. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
3M Dyneon™ PFA 6503 C EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6503 C EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick .. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | 2mm/min; ASTM D790-86 |
Micropol Microcene MC121 Metallocene Based Polyethylene Rotational Molding Powder Characteristics: reduced fusion, compacting, and crystallization times or lower oven temperatures; improved wall thickness control, improved impact resistance; low warpage; better creep resistance. .. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D760-66 |
Micropol Microlin ML91 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | Tangent at 0.05 in/min; ASTM D790A |
LyondellBasell Hifaxâ„¢ ETA-3081 Thermoplastic Olefin Resin Key Features: medium high melt flow, medium modulus, paintable thermoplastic olefin resin, excellent balance of properties, excellent processability, good paintability and paint durability, good sur.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ISO 178 |
LyondellBasell Hifaxâ„¢ ETA-3104HF Thermoplastic Olefin Resin Key Features: medium melt flow, medium modulus thermoplastic elastomeric olefin resin, good impact and stiffness balance, good dimensional stability, good processabilityApplications: molded-in color.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
Sumitomo Chemical ESPOLEX® 903 Thermoplastic Elastomer ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | 50% humidity; ISO 178 |
Borealis Bormed™ SC820CF Polypropylene Random Copolymer Bormed™ SC820CF is a very soft random heterophasic copolymer. Applications: Bormed™ SC820CF is recommended for packaging for medical devices. Bormed™ SC820CF contains no slip, antiblock, antist.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ISO 178 |
Borealis Borseal™ RE939CF Polypropylene Copolymer Borseal™ RE939CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: Borseal™ RE939CF is designed for: Food packaging,.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
Tipco Tipcolene® TPE-HMI TPE HMI - Impact Modified Polypropylene Copolymer Compound with High Flow, Soft Touch High Impact PP CopolymerApplications: Automotive BumpersProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 0.550 GPa | 79.7 ksi | 1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A |
Dow DS6D81 Polypropylene Resin DOW DS6D81 is intended for use as a heat seal coating on oriented polypropylene (OPP) film.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Flexural Modulus | 0.550 GPa | 79.7 ksi | 1% Secant; molded and tested in accordance with ASTM D 4101; ASTM D790A |
Dow DS6D82 Polypropylene Resin DOW DS6D82 is intended for use as a heat seal coating on oriented polypropylene (OPP) film.Information provided by DowDow Announced Sale of Global Polypropylene Business to Braskem in July 2011. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | 50%RH; ISO 178 |
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6
(Unverified Data**) Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide .. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | SAE J949 |
Azdel SuperLite® SL551600-100 PP Resin Matrix / 55% Glass Fiber (7 mm Molded Thickness) AZDEL SuperLite® SL551600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
3M Dyneon™ PFA 6502 TAZ Perfluoroalkoxy Fluorothermoplastic Granules 3M™ Dyneon™ PFA 6502TAZ is a fluorothermoplastic resin for compression molding applications. PFA 6502TAZ has a wide processing window with excellent color stability when longer residence times or .. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | |
3M Dyneon™ PFA 6502 UHPZ Perfluoroalkoxy Fluorothermoplastic Granules Dyneon PFA X 6502 UPH, PFA X 6505 UHP and PFA X 6515 UHP are a new series of ultra-high purity fluorothermoplastics. These resins were developed for high-purity applications requiring ultra-low leve.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
3M Dyneon™ PFA 6502TZ Perfluoroalkoxy Fluorothermoplastic Granules 3M™ Dyneon™ PFA 6502TZ is a fluorothermoplastic resin for transfer molding applications and extrusion of claddings and linings. Dyneon PFA 6502TZ allows for easy processing under low shear rates, .. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
3M Dyneon™ PFA 6503PAZ Fluoroplastic Powder 3M™ Dyneon™ Fluoroplastic Powder PFA 6503PAZ is a fluorothermoplastic powder designed for use in thin film powder coatings. Typical applications include non-stick surfaces, chemical vessel and tan.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
3M Dyneon™ PFA 6503PBZ Fluoroplastic Powder 3M™ Dyneon™ Fluoroplastic Powder PFA 6503PBZ is a fluorothermoplastic powder with excellent thermal stability characteristics, designed for use in thin film powder coatings. Typical applications i.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | Injection Molded Bars (0.5"x.125"x 5"); ASTM D790 |
3M Dyneon™ PFA 6505TZ Fluoroplastic Granules 3M™ Dyneon™ Fluoroplastic Granules PFA 6505TZ (a fully fluorinated copolymer of tetrafluoroethylene and perfluorovinylether) has exceptional temperature resistance, excellent electrical properties.. |
|||
Flexural Modulus | 0.550 GPa | 79.8 ksi | ASTM D790 |
3M Dyneon™ PFA 6503 B EPC Perfluoroalkoxy Fluorothermoplastic
(discontinued **) Dyneon PFA 6503 B EPC is a fluorothermoplastic powder for powder coating applications, and is designed for thin film applications where target film thickness is 25-40 micrometers per pass.non-stick .. |
|||
Flexural Modulus | 0.550 - 2.28 GPa | 79.8 - 331 ksi | Average value: 1.38 GPa Grade Count:141 |
Overview of materials for Polypropylene, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Film Grade". Each property range of values reported is minimum and maximum values of appr.. |