Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Flexural Modulus = 0.415 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.415 GPa
60.2 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Flexural Modulus 0.415 GPa
60.2 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Flexural Modulus 0.415 GPa
60.2 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Flexural Modulus 0.415 GPa
60.2 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Flexural Modulus 0.415 GPa
60.2 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Flexural Modulus 0.415 GPa
60.2 ksi
ASTM D790
A. Schulman POLYFORT™ PP 3720
Information provided by A. Schulman.
Flexural Modulus 0.415 GPa
60.2 ksi
MD; ASTM D790
DuPont™ Nomex® Type 994, 250 mil Nominal Thickness Rigid Aromatic Nylon Board
Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T..
Flexural Modulus 0.415 GPa

@Temperature 65.0 °C
60.2 ksi

@Temperature 149 °F
ASTM Test
BASF Ultramid® 8253 HS PA6 (Dry)
Ultramid 8253 HS is a heat stabilized, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications requiring improved dry as molded toughness and increased..
Flexural Modulus 0.415 GPa

@Temperature 65.0 °C
60.2 ksi

@Temperature 149 °F
ASTM Test
BASF Ultramid® 8253 PA6 (Dry)
Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o..
Copyright © lookpolymers.com All Rights Reserved