Mechanical Properties Metric English Comments
Flexural Modulus 0.360 - 0.440 GPa
52.2 - 63.8 ksi
2 mm/min; ASTM D790
Solvay Specialty Polymers Solef® 21508 PVDF Copolymer  (discontinued **)
Key features of this grade: High Elongation, Wire & Cable, Plenum, Formulated. Recommended processing is extrusion. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® P..
Flexural Modulus 0.360 GPa
52.2 ksi
ASTM D 790
SABIC Innovative Plastics LNP Stat-kon TD000
LNP* Stat-kon* TD000 is a compound based on Polyurethane resin. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 0.360 GPa
52.2 ksi
ASTM D790
SABIC Innovative Plastics LNP STAT-KON TD000 PU
LNP* STAT-KON* TD000 is an unfilled compound based on Polyurethane resin. Added feature of this material is: Electrically Conductive.
Flexural Modulus 0.360 GPa
52.2 ksi
ASTM D790
Sumitomo Chemical ESPOLEX® 817 Thermoplastic Elastomer
ESPOLEX® TPE Series is a group of thermoplastic elastomers produced by Sumitomo Chemical Company. Among its material advantages, ESPOLEX® TPE Series is distinguished by offering many low-densi..
Flexural Modulus 0.360 GPa
52.2 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Flexural Modulus 0.360 GPa
52.2 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Flexural Modulus 0.360 GPa
52.2 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Flexural Modulus 0.360 GPa
52.2 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Flexural Modulus 0.360 GPa
52.2 ksi
ASTM D790
UBE PAE1201U Nylon Elastomer
Description: UBESTA Nylon 12 ElastomerInformation provided by UBE.
Flexural Modulus 0.360 GPa
52.2 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Flexural Modulus 0.360 GPa
52.2 ksi
MD; ASTM D790
DuPont™ Nomex® Type 994, 125 mil Nominal Thickness Rigid Aromatic Nylon Board
Type 994 is a densified, rigid board which has a unique combination of superior resistance to compression, even at elevated temperatures, along with relatively high oil absorption characteristics. T..
Flexural Modulus 0.360 - 0.440 GPa
52.2 - 63.8 ksi
2 mm/min; ASTM D790
Solvay Specialty Polymers Solef® 20810 PVDF Copolymer  (discontinued **)
Key features of this grade: Li Battery, Virgin. Recommended processing is solution. Available as powder & granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorinated semi-crysta..
Flexural Modulus 0.360 GPa
52.2 ksi
Conditioned 15 days at 23°C - 50% RH; ISO178
Arkema Group Pebax® Rnew 70R53 SP 01 Polyether Block Amide (PEBA)
Polyether block amide Pebax® 70R53 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide based on renewable resources. This SP grade has been developed to be heat and UV..
Flexural Modulus 0.360 GPa
52.2 ksi
Tangent; ISO 178
A. Schulman FORMION™ FI 105E Non-Reinforced, Extrusion Grade Sodium Ionomer
DescriptionFormion® FI 1051E is a non-reinforced, transparent, extrusion grade Sodium Ionomer. It has been formulated for high durability, cut and puncture resistance, and low temperature ductilit..
Flexural Modulus 0.360 GPa
52.2 ksi
ASTM D790
C.O.I.M. LARIPUR® LPR6520 Standard Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..