Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.327 GPa | 47.4 ksi | |
Dow DOWLEX™ 2535 Linear Low Density Polyethylene, Narrow MW Distribution DOWLEX® 2535 Polyethylene resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and stress crack resistance with good flexibility. It has good proces.. |