Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.285 GPa
41.3 ksi
Conditioned 15 days at 23°C - 50% RH; ISO 178
Arkema Group Pebax® 6333 SA 01 MED Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SA 01 MED is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This grade offers the highest quality and it is specially designed to meet t..
Flexural Modulus 0.285 GPa
41.3 ksi
Conditioned 15 days at 23°C - 50% RH; ISO178
Arkema Group Pebax® 6333 SA 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SA 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SA grade is specially designed to food uses.Information provided by Arkema ..
Flexural Modulus 0.285 GPa
41.3 ksi
Conditioned 15 days at 23°C - 50% RH; ISO178
Arkema Group Pebax® 6333 SP 01 Polyether Block Amide (PEBA)
Polyether block amide PEBAX® 6333 SP 01 is a thermoplastic elastomer made of flexible polyether and rigid polyamide. This SP grade has been developed to be heat and UV resistant.Information provide..