Mechanical Properties Metric English Comments
Flexural Modulus 0.234 GPa
33.9 ksi
method 1, Proc.B; ASTM D-790
Multibase Multi-Flex® TPE D 4502 BLK
Multi-Flex® D 4502 is based on Shell's Kraton G polymer and is suitable for applications for the automotive industry. It exhibits excellent paintability adhesion and is recommended as substrate fo..
Flexural Modulus 0.234 GPa
33.9 ksi
2% Secant, 12.7 mm/min; ASTM D790
Eastman D4027-P Voridian Polyethylene  (discontinued **)
VORIDIAN low density polyethylene D4027-P is a formulation suggested for extrusion coating applications that require clarity, high gloss and superior hot tack properties. Applications/UsesFood Packa..
Flexural Modulus 0.234 GPa
34.0 ksi
1% Secant; ASTM D790
Multibase Multi-Flex® D 3902 MRS TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Flexural Modulus 0.234 GPa
34.0 ksi
ASTM D790
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Blow Molding)
ApplicationsPETROTHENE NA 940-000 is a low density homopolymer resin intended for use in blow molding applications. Excellent toughness, good clarity and processability make NA 940-000 an ideal cho..
Flexural Modulus 0.234 GPa
34.0 ksi
Molded; ASTM D790
LyondellBasell Petrothene® NA940085 Low Density Polyethylene (Film Grade)
ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for..
Flexural Modulus 0.234 GPa
34.0 ksi
Molded; ASTM D790
LyondellBasell Petrothene® NA940094 Low Density Polyethylene (Film Grade)
ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for..
Flexural Modulus 0.234 GPa
33.9 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass)
Information provided by A. Schulman.
Flexural Modulus 0.234 GPa
33.9 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass)
Information provided by A. Schulman.
Flexural Modulus 0.234 GPa
33.9 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass)
Information provided by A. Schulman.
Flexural Modulus 0.234 GPa
33.9 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass)
Information provided by A. Schulman.
Flexural Modulus 0.234 GPa
33.9 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass)
Information provided by A. Schulman.
Flexural Modulus 0.234 GPa
33.9 ksi
1.3 mm/min; ASTM D790
A. Schulman POLYPUR™ FPU 1112 Thermoplastic Polyurethane Compound (15% Glass)
Information provided by A. Schulman.
Flexural Modulus 0.234 GPa
34.0 ksi
2% Secant; Molded and tested in accordance with ASTM D4976; ASTM D790 B
Dow 722 Linear Low Density Polyethylene (LDPE)
DOW Polyethylene 722 is a broad molecular weight distribution homopolymer designed to offer good impact strength and rack resistance, with excellent flexibility. Typical applications include caps/c..
Flexural Modulus 0.234 GPa
34.0 ksi
ASTM D790
Lubrizol ESTANE® 58142 Ester Based Thermoplastic Polyurethane
Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Flexural Modulus 0.234 - 45.0 GPa
33.9 - 6530 ksi
Average value: 9.38 GPa Grade Count:74
Overview of materials for Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Glass Fiber Reinforced". Each property range of values reported is mi..
Flexural Modulus 0.234 GPa
34.0 ksi
Molded; ASTM D790
LyondellBasell Petrothene® NA940000 Low Density Polyethylene (Film Grade)
ApplicationsPETROTHENE NA 940 is a series of resins designed for heavy duty film applications. Superior puncture resistance combined with excellent impact properties make NA 940 an ideal choice for..