Mechanical Properties Metric English Comments
Flexural Modulus 0.221 GPa
32.1 ksi
ISO 178/1A
Radici Heraflex® E 5620 TPC-ET Thermoplastic Elastomer
TPC-ET Thermoplastic Elastomer. Medium Modulus, Nominal Shore D/15s 50. Natural colorProcessing technology: Injection moldingInformation provided by Radici group.
Flexural Modulus 0.221 GPa
32.1 ksi
2% Secant; ASTM D 790
Eastman Tenite Polyethylene 1810A Low Density Polyethylene - Molding  (discontinued **)
Product Description: TENITE Polyethylene 1810A contains NO ADDITIVES. It is suggested for injection molding applications. TENITE Polyethylene 1810A meets the requirements of FDA regulation 21 CFR 1..
Flexural Modulus 0.221 GPa
32.1 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 1810A Polyethylene  (discontinued **)
Polyethylene 1810A contains no additives. It is suggested for injection molding applications.Information from manufacturer data sheet.Eastman Chemical Company sold its polyethylene business to West..
Flexural Modulus 0.221 GPa
32.1 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 1810E Polyethylene  (discontinued **)
Polyethylene 1810E contains no additives. It is suggested for general purpose extrusion applications requiring good stress crack resistance or electrical properties. It is used in applications suc..
Flexural Modulus 0.221 GPa
32.1 ksi
2% Secant, 12.7 mm/min. (0.5 in./min.); ASTM D790
Eastman 18DOA Polyethylene  (discontinued **)
Polyethylene 18DOA is a low density formulation suggested for the production of closures where a high melt index material is needed to meet shrinkage requirements and fast molding cycles. It molds ..
Flexural Modulus 0.221 GPa
32.1 ksi
ASTM D790
Lubrizol Pellethane® 2363-65D Thermoplastic Polyurethane Elastomer
Feature: USP Class VIAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009.
Flexural Modulus 0.221 GPa
32.1 ksi
3 pt. Tangent; ASTM D790
Chevron Phillips Marlex® 1122B Injection Molding Resin
Resin Type: Homopolymer; ASTM D 4976 Classification: PE 113, A 24200Characteristics: Excellent Flexibility, Moderate Flow, Moderate Warping Resistance, Moderate Mold Release, Excellent ESCRApplicati..
Flexural Modulus 0.221 - 0.345 GPa
32.0 - 50.0 ksi
ASTM D790
Buckeye Polymers BP FLEX D4107 GO1 BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..