Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.175 GPa | 25.4 ksi | ASTM D790 |
ExxonMobil Iotek® 7020 Zinc Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A zinc ionomer with excellent flexibility, abrasion resistance, impact strength and tensile strength. This ionomer has outstanding adhesion to glas.. |