Mechanical Properties Metric English Comments
Flexural Modulus 0.120 GPa
17.4 ksi
ASTM D790
Rotuba H Cellulose Acetate
Property values at 50% RH.Data provided by the manufacturer.
Flexural Modulus 0.120 GPa
17.4 ksi
ISO 178
Polimeri Europa Riblene® MQ 10 Low Density Polyethylene - Injection Molding
Riblene MQ 10 is a good fluidity low density polyethylene resin (LDPE).Parts made with Riblene MQ 10 are characterized by a high flexibility.Main Applications: Riblene MQ 10 is suitable for injecti..
Flexural Modulus 0.120 GPa
17.4 ksi
ISO 178
Polimeri Europa Riblene® MQ 10 R Low Density Polyethylene - Injection Molding
Riblene MQ 10 R is a good fluidity low density polyethylene resin (LDPE).Parts made with Riblene MQ 10 R are characterized by a high flexibility.Main Applications: Riblene MQ 10 R is suitable for i..
Flexural Modulus 0.120 GPa
17.4 ksi
ISO 178
Polimeri Europa Riblene® MR 10 Low Density Polyethylene - Injection Molding
Riblene MR 10 is a high fluidity low density polyethylene resin (LDPE).Parts made with Riblene MR 10 are characterized by a high flexibility.Main Applications: Riblene MR 10 is suitable for injecti..
Flexural Modulus 0.120 GPa
17.4 ksi
ISO 178
Polimeri Europa Riblene® MR 10 R Low Density Polyethylene - Injection Molding
Riblene MR 10 R is a high fluidity low density polyethylene resin (LDPE).Parts made with Riblene MR 10 R are characterized by a high flexibility.Main Applications: Riblene MR 10 R is suitable for i..
Flexural Modulus 0.120 GPa
17.4 ksi
ASTM D790
Covestro Texin® DP7-3008 Thermoplastic Polyurethane, Polyester-based, Aliphatic  (discontinued **)
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ..
Flexural Modulus 0.120 GPa
17.4 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP PDXF89080 PE
LNP* LUBRICOMP* PDXF89080 is a compound based on Polyethylene containing Proprietary Fillers. Added feature of this grade is: Wear Resistant.
Flexural Modulus 0.120 GPa
17.4 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP PDXF89080 PE
LNP* LUBRICOMP* PDXF89080 is a compound based on Polyethylene containing Proprietary Fillers. Added feature of this grade is: Wear Resistant.
Flexural Modulus 0.120 GPa
17.4 ksi
ISO 178
Chengdu Polyster H5550 Thermoplastic Polyether-ester Elastomer (TPEE)
Medium-low modulus molding and injection grade. Contains improved color- stable antioxidants. Good balance of low and high temperature properties. Applications requiring high original color retentio..
Flexural Modulus 0.120 GPa
17.4 ksi
ISO 178
Chengdu Polyster H5550B Thermoplastic Polyether-ester Elastomer (TPEE)
Low modulus molding and extrusion grade. Contains color-stable antioxidants. Good balance of low and high temperature properties. Excellent flex-fatigue resistance. Excellent creep resistance. CVJ b..
Flexural Modulus 0.120 GPa
17.4 ksi
ASTM D638
Arkema Group LOTADER® 3200 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3200 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized under high pressure in an autoclave process. Due to its properties, LOTADER 3200 is used in pipeline ..
Flexural Modulus 0.120 GPa
17.4 ksi
ASTM D638
Arkema Group LOTADER® 3210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 3210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. Main applicationsLOTADER 3210 is a versatile adhesive for extrusi..
Flexural Modulus 0.120 GPa
17.4 ksi
ASTM D638
Arkema Group LOTADER® 4210 Terpolymer Ethylene - Acrylic Ester - Maleic Anhydride
LOTADER 4210 is a random terpolymer of Ethylene, Acrylic Ester and Maleic Anhydride, polymerized by high-pressure autoclave process. LOTADER 4210 is a versatile adhesive for extrusion coating or lam..