Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.115 GPa | 16.7 ksi | ISO 178 |
Polimeri Europa Clearflex® MQ B0 Very Low Density Polyethylene Clearflex MQ B0 is a linear polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin shows an excellent balance between flexibility and impact resistance.Main Applicati.. |
|||
Flexural Modulus | 0.115 GPa | 16.7 ksi | ASTM D790 |
C.O.I.M. LARIPUR® LPR5225 Special Adipate Ester Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |