Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0785 GPa @Thickness 6.40 mm |
11.4 ksi @Thickness 0.252 in |
15mm/min; ASTM D790 |
LG Chemical KEYFLEX BT 1045D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, Medium ModulusApplication: Antenna Cover, Injection Parts for Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |