Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0100 GPa | 1.45 ksi | ISO 178 |
Polimeri Europa Greenflex® ML 60 Ethylene Vinyl Acetate Copolymer - Injection Molding, Compounding & Extrusion Greenflex ML 60 is an ethylene vinyl acetate copolymer (EVA) for injection molding, compounding and extrusion. Items produced with Greenflex ML 60 show very high elasticity.Main Applications: Gree.. |
|||
Flexural Modulus | 0.0100 - 51.7 GPa | 1.45 - 7500 ksi | Average value: 5.34 GPa Grade Count:212 |
Overview of materials for Nylon 12 This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12". Each property range of values reported is minimum and maximum values of appropriate MatWeb en.. |
|||
Flexural Modulus | 0.0100 GPa | 1.45 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East) Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 0.0100 GPa @Temperature 49.0 °C |
1.45 ksi @Temperature 120 °F |
ASTM D790 |
DuPont Elvax® 260 Ethylene-Vinyl Acetate Copolymer Resin Elvax resins offer a unique combination of processing and performance characteristics. They provide outstanding toughness and resilience and maintain flexibility over a broad temperature range with.. |
|||
Flexural Modulus | 0.0100 GPa | 1.45 ksi | ASTM D638 |
Arkema Group LOTRYL® 28 MA 07 Copolymer Ethylene - Methyl Acrylate LOTRYL® 28 MA 07 is a random copolymer of ethylene and methyl acrylate made by high-pressure radicalar polymerisation process. Due to the high methyl acrylate content, LOTRYL® 28 MA 07 is a polyme.. |