Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.00190 - 0.345 GPa | 0.276 - 50.0 ksi | Average value: 0.0630 GPa Grade Count:62 |
Overview of materials for Ethylene Vinyl Acetate Copolymer (EVA), Molded/Extruded This property data is a summary of similar materials in the MatWeb database for the category "Ethylene Vinyl Acetate; Molded/Extruded". Each property range of values reported is minimum and maximum .. |