Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 7.35 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched >= 3.92 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
>= 7.35 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ISO 180
LG Chemical EM500 Impact modifier for Engineering Plastics
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi..
Izod Impact, Unnotched >= 3.92 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
>= 7.35 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ISO 180
LG Chemical EM500A Impact modifier for Engineering Plastics
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi..
Izod Impact, Unnotched >= 3.92 J/cm

@Thickness 3.17 mm,
Temperature -30.0 °C
>= 7.35 ft-lb/in

@Thickness 0.125 in,
Temperature -22.0 °F
ISO 180
LG Chemical EM505 Impact modifier for Engineering Plastics
Description: LG Chem impact modifiers for Engineering Plastic are developed to enhance the impact strength of Engineering Plastics (PC, PBT, ABS, PC/PBT, PC/ABS, etc). LG Chem has 2 type impact modi..