Polymer Property : Izod Impact, Unnotched = 37.11 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 19.81 J/cm

@Temperature 23.0 °C
37.11 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Noryl PX4058 PPE+PS
PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 19.81 J/cm

@Temperature 23.0 °C
37.11 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics Noryl PX4058 PPE+PS (Asia Pacific)
PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Asia Pacific region.