Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 19.81 J/cm @Temperature 23.0 °C |
37.11 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 19.81 J/cm @Temperature 23.0 °C |
37.11 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Noryl PX4058 PPE+PS (Asia Pacific) PPO, polyolefin blend. Improved chemical resistance. 253F (125C) HDT.This data was supplied by SABIC-IP for the Asia Pacific region. |