Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 58.0 GPa @Temperature 23.0 °C |
8410 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® M26/M26T 120°C (250°F) Curing Epoxy Matrix, M26/45%/G1070 Carbon Fabric 6K T300J 370 gsmInformation provided by HexCel |