Polymer Property : Flexural Modulus = 4.50 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 4.50 GPa

@Temperature 23.9 °C
653 ksi

@Temperature 75.0 °F
ASTM D790
Saint-Gobain Meldin® 7022 DF Direct Formed Graphite Filled Polyimide
Melidin® 7022 DF is a direct formed polyimide that contains 40% graphite filler. This grade offers additional dimensional stability at elevated temperatures and the lowest CTE of any Meldin® ..
Flexural Modulus 4.50 GPa

@Temperature 80.0 °C
653 ksi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-402 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 4.50 GPa

@Temperature 80.0 °C
653 ksi

@Temperature 176 °F
Practical Use (Water Absorption 2.0%); ASTM-D790
Toyobo GLAMIDE® T-403 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 4.50 GPa

@Temperature -40.0 °C
653 ksi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-502NZ 6T-Nylon
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..