Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.14 GPa @Temperature 23.0 °C |
310 ksi @Temperature 73.4 °F |
DAM; ASTM D790 |
DuPont Performance Polymers Zytel® FE3734 NC010 Nylon 612