Polymer Property : Flexural Modulus = 2.76 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.76 GPa

@Temperature -40.0 °C
400 ksi

@Temperature -40.0 °F
50%RH; ASTM D790
DuPont Performance Polymers Zytel® 158L NC010 Nylon 612  (Unverified Data**)
Zytel® 158L NC010 is an intermediate viscosity, lubricated polyamide 612 resin that is suitable for molding and extrusion applications.Information provided by DuPont Performance Polymers
Flexural Modulus 2.76 GPa

@Temperature 260 °C
400 ksi

@Temperature 500 °F
ASTM D790
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Machined Parts
Higher abrasion resistance than G15, high value stability and very low friction coefficient propertyInformation provided by Daelim H&L
Flexural Modulus 2.76 GPa

@Temperature -40.0 °C
400 ksi

@Temperature -40.0 °F
ASTM D790
BASF Ultramid® 8281 HS GP PA6 (Dry)
Description: Ultramid 8281 HS GP is an unreinforced, heat stabilized PA6 rot molding compound. It is available in natural and black and can be painted. It exhibits excellent balance of engineering p..