Polymer Property : Flexural Modulus = 2.70 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 2.70 GPa

@Temperature 40.0 °C
392 ksi

@Temperature 104 °F
Hybrid Plastics CO6U50.02 Nanoreinforced® Cyclic Olefin Copolymer
Impact modified, flame retardantThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where l..
Flexural Modulus 2.70 GPa

@Temperature 23.9 °C
392 ksi

@Temperature 75.0 °F
ASTM D790
Saint-Gobain Meldin® 7211 DF Direct Formed Graphite and PTFE Filled Polyimide
Melidin® 7211 DF is a direct formed polyimide that contains 15% graphite and 10% PTFE fillers. This grade has the lowest coefficient of friction of the Meldin® 7000 series polyimides.Specific..
Flexural Modulus 2.70 GPa

@Temperature 23.0 °C
392 ksi

@Temperature 73.4 °F
Practical Use (Water Absorption 3.0%); ASTM-D790
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 2.70 GPa

@Temperature 23.0 °C
392 ksi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-656E Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 2.70 GPa

@Temperature -40.0 °C
392 ksi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® TY-102ND Nylon/Elastomer
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 2.70 GPa

@Temperature 23.0 °C
392 ksi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-802 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..