Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 123 GPa @Temperature 232 °C |
17800 ksi @Temperature 450 °F |
1255 Hrs |
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |
|||
Flexural Modulus | 123 GPa @Temperature 232 °C |
17800 ksi @Temperature 450 °F |
1608 Hrs |
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |
|||
Flexural Modulus | 123 GPa @Temperature 23.0 °C |
17800 ksi @Temperature 73.4 °F |
|
Hexcel® HexPly® F650 Bismaleimide Resin with T300 Fiber Thermal Aging at 232°C; Composition T300 Fiber, 6K, UD Tape - 148 g/m2; Laminate Physicals: 32.7% Resin content, 60.0% Fiber volumeInformation provided by HexCel |