Mechanical Properties Metric English Comments
Flexural Modulus 1.70 GPa

@Temperature 23.0 °C
247 ksi

@Temperature 73.4 °F
DAM; ISO 178
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Zytel® ST7301 NC010 is a Super Tough, heat stabilized, lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide temperature and humidity..
Flexural Modulus 1.70 GPa

@Temperature 130 °C
247 ksi

@Temperature 266 °F
Hybrid Plastics CO6U50.01 Nanoreinforced® Cyclic Olefin Copolymer
Impact modified, UV stabilizedThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where low..
Flexural Modulus 1.70 GPa

@Temperature 130 °C
247 ksi

@Temperature 266 °F
Hybrid Plastics CO6U50.02 Nanoreinforced® Cyclic Olefin Copolymer
Impact modified, flame retardantThe exceptional heat distortion temperature and low density of cyclic olefin copolymers (COC) makes them excellent materials for high temperature applications where l..
Flexural Modulus 1.70 GPa

@Temperature 260 °C
247 ksi

@Temperature 500 °F
ASTM D790
Saint-Gobain Meldin® 7001 CM Compression Molded Polyimide
Meldin® 7001 CM unfilled polyimide base resin, compression moldedSpecification Qualifications:Satisfies Type I P for ASTM D 6456-99: Standard Specification for Finished Parts Made from Polyimide ..
Flexural Modulus 1.70 GPa

@Temperature 80.0 °C
247 ksi

@Temperature 176 °F
Practical Use (Water Absorption 3.0%); ASTM-D790
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 1.70 GPa

@Temperature 80.0 °C
247 ksi

@Temperature 176 °F
Practical Use (Water Absorption 2.3%); ASTM-D790
Toyobo GLAMIDE® T-422-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 1.70 GPa

@Temperature 80.0 °C
247 ksi

@Temperature 176 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-777-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Modulus 1.70 GPa

@Temperature 150 °C
247 ksi

@Temperature 302 °F
ISO 178
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..