Mechanical Properties Metric English Comments
Gardner Impact 25.0 J

@Temperature 23.0 °C
18.4 ft-lb

@Temperature 73.4 °F
ASTM D3029
LyondellBasell Hostacomâ„¢ CB189FC/1 Thermoplastic Polyolefin Elastomer
Description: Hostacomâ„¢ CB189FC/1 medium melt flow, 1,300 MPa flexural modulus, precolored, mineral-filled thermoplastic elastomeric olefin (TEO) resin has a very good balance of impact, stiffne..
Gardner Impact 25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
ASTM D3029
SABIC Innovative Plastics NORYL HN731A PPE+PS
PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine..
Gardner Impact 25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
ASTM D3029
SABIC Innovative Plastics NORYL 731 PPE+PS
PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi..
Gardner Impact 25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
ASTM D 3029
SABIC Innovative Plastics Noryl 731H PPE+PS
High gloss, general purpose grade. 130C (266F) DTUL. UL 94 HB rated. For multiple plugs, wine filter plates, etc.This data was supplied by SABIC-IP for the Americas region.
Gardner Impact 25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
ASTM D 3029
SABIC Innovative Plastics Noryl EN212 PPE+PS
Extrusion grade. 212F (100C) DTUL. UL94 V-1 rated.This data was supplied by SABIC-IP for the Americas region.
Gardner Impact 25.0 J

@Temperature -30.0 °C
18.4 ft-lb

@Temperature -22.0 °F
ASTM D3029
SABIC Innovative Plastics NORYL ENG265 PPE+PS
PPE+PS blend. Unfilled. Suitable for profile extrusion. NSF listed for potable water use in several colors (Standard 61). Low water absorption. Hydrolytic stability. Dimensional stability. Typical a..