Polymer Property : Gardner Impact = 10.0 ft-lb Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Gardner Impact 13.6 J

@Temperature 23.0 °C
10.0 ft-lb

@Temperature 73.4 °F
ASTM D5420
Noble Polymers Regis™ 125098 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Gardner Impact 13.6 J

@Temperature -30.0 °C
10.0 ft-lb

@Temperature -22.0 °F
ASTM D5420
Noble Polymers Regis™ 155120 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Gardner Impact 13.6 J

@Temperature 23.0 °C
10.0 ft-lb

@Temperature 73.4 °F
ASTM D5420
Noble Polymers Regis™ 155120 Thermoplastic Olefin (TPO)
Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi..
Gardner Impact 13.6 J

@Temperature 22.8 °C
10.0 ft-lb

@Temperature 73.0 °F
ASTM D5420
Spartech EP6120 Filled and Reinforced Copolymer
Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength..
Gardner Impact 13.6 J

@Temperature 22.8 °C
10.0 ft-lb

@Temperature 73.0 °F
ASTM D5420
Spartech EP6430 Filled and Reinforced Copolymer
Filled copolymers offer a higher level of impact performance than homopolymer materials, and higher stiffness than unfilled copolymers. Copolymer based materials retain much of their impact strength..