Polymer Property : Dart Drop, Total Energy = 99.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 99.0 J

@Temperature 0.000 °C
73.0 ft-lb

@Temperature 32.0 °F
ASTM D3763
SABIC Innovative Plastics ULTEM DH1004 PEI
Dart Drop, Total Energy 99.0 J

@Temperature 0.000 °C
73.0 ft-lb

@Temperature 32.0 °F
ASTM D3763
SABIC Innovative Plastics ULTEM DH1004 PEI (Asia Pacific)
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability.
Dart Drop, Total Energy 99.0 J

@Temperature 0.000 °C
73.0 ft-lb

@Temperature 32.0 °F
ASTM D3763
SABIC Innovative Plastics ULTEM DH1004 PEI (Europe-Africa-Middle East)
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. RoHS compliant and UL94 V0 listed.
Dart Drop, Total Energy 99.0 J

@Temperature 0.000 °C
73.0 ft-lb

@Temperature 32.0 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU1004 PEI
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocomp..
Dart Drop, Total Energy 99.0 J

@Temperature 0.000 °C
73.0 ft-lb

@Temperature 32.0 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU1004 PEI (Asia Pacific)
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f..
Dart Drop, Total Energy 99.0 J

@Temperature 0.000 °C
73.0 ft-lb

@Temperature 32.0 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East)
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f..
Dart Drop, Total Energy 99.0 J

@Temperature 0.000 °C
73.0 ft-lb

@Temperature 32.0 °F
ASTM D3763
SABIC Innovative Plastics ULTEM 9090 PEI
Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution.
Dart Drop, Total Energy 99.0 J

@Temperature 0.000 °C
73.0 ft-lb

@Temperature 32.0 °F
ASTM D3763
SABIC Innovative Plastics ULTEM 9090 PEI (Europe-Africa-Middle East)
Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution.