Polymer Property : Dart Drop, Total Energy = 93.0 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 93.0 J

@Temperature 23.0 °C
68.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU1004 PEI
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocomp..
Dart Drop, Total Energy 93.0 J

@Temperature -20.0 °C
68.6 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU1004 PEI
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. For medical devices and pharmaceutical applications. Healthcare management of change, biocomp..
Dart Drop, Total Energy 93.0 J

@Temperature 23.0 °C
68.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU1004 PEI (Asia Pacific)
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f..
Dart Drop, Total Energy 93.0 J

@Temperature -20.0 °C
68.6 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU1004 PEI (Asia Pacific)
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f..
Dart Drop, Total Energy 93.0 J

@Temperature 23.0 °C
68.6 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East)
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f..
Dart Drop, Total Energy 93.0 J

@Temperature -20.0 °C
68.6 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East)
High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f..