Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® XCY620HS PC+ABS PC+ ABS General Purpose Non-FR |
|||
Dart Drop, Total Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS PC+ ABS Automotive applications |
|||
Dart Drop, Total Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Asia Pacific) PC+ ABS Automotive applications |
|||
Dart Drop, Total Energy | 65.0 J @Temperature -30.0 °C |
47.9 ft-lb @Temperature -22.0 °F |
ASTM D3763 |
SABIC Innovative Plastics Cycoloy® XCY620S PC+ABS (Europe-Africa-Middle East) PC+ ABS automotive applications, excellent flow/impact balance, high heat resistance temperature and excellent properties retention after hydrolytic and heat aging. |