Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Dart Drop, Total Energy | 88.0 J @Temperature 23.0 °C |
64.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM DH1004 PEI |
|||
Dart Drop, Total Energy | 88.0 J @Temperature -20.0 °C |
64.9 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM DH1004 PEI |
|||
Dart Drop, Total Energy | 88.0 J @Temperature 23.0 °C |
64.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Asia Pacific) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. |
|||
Dart Drop, Total Energy | 88.0 J @Temperature -20.0 °C |
64.9 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Asia Pacific) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. |
|||
Dart Drop, Total Energy | 88.0 J @Temperature 23.0 °C |
64.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. RoHS compliant and UL94 V0 listed. |
|||
Dart Drop, Total Energy | 88.0 J @Temperature -20.0 °C |
64.9 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM DH1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. RoHS compliant and UL94 V0 listed. |
|||
Dart Drop, Total Energy | 88.0 J @Temperature 23.0 °C |
64.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 9090 PEI Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution. |
|||
Dart Drop, Total Energy | 88.0 J @Temperature -20.0 °C |
64.9 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 9090 PEI Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution. |
|||
Dart Drop, Total Energy | 88.0 J @Temperature 23.0 °C |
64.9 ft-lb @Temperature 73.4 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 9090 PEI (Europe-Africa-Middle East) Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution. |
|||
Dart Drop, Total Energy | 88.0 J @Temperature -20.0 °C |
64.9 ft-lb @Temperature -4.00 °F |
ASTM D3763 |
SABIC Innovative Plastics ULTEM 9090 PEI (Europe-Africa-Middle East) Polyetherimide Blend with improved Ductility and Detergent resistance. Meets FAR 25.853 and OSU 55/55 heat release and provides low toxicity, smoke and flame evolution. |