Mechanical Properties Metric English Comments
Dart Drop, Total Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4850 PBT+PC
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Dart Drop, Total Energy 60.0 J

@Temperature -20.0 °C
44.3 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4850 PBT+PC
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Dart Drop, Total Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Dart Drop, Total Energy 60.0 J

@Temperature -20.0 °C
44.3 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Europe-Africa-Middle East)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Dart Drop, Total Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Dart Drop, Total Energy 60.0 J

@Temperature -20.0 °C
44.3 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Asia Pacific)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Dart Drop, Total Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Dart Drop, Total Energy 60.0 J

@Temperature -20.0 °C
44.3 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4870HH PC+PET (Europe-Africa-Middle East)
Xenoy X4870HH is a high heat, very high modulus and ductile PC/PET blend. Furthermore this resin provides chemical resistance, very low creep, low CTE, excellent fatique and high heat dimensional st..
Dart Drop, Total Energy 60.0 J

@Thickness 3.20 mm,
Temperature 23.0 °C
44.3 ft-lb

@Thickness 0.126 in,
Temperature 73.4 °F
Injection Molded, Total Energy; ASTM D3763
Styron EMERGEâ„¢ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET)
Overview: EMERGEâ„¢ PC/PET 9500 CR advanced resin is a polycarbonate blend with excellent chemical resistance and ignition resistance properties. This grade was designed for use in medical equipm..
Dart Drop, Total Energy 60.0 J

@Temperature 23.0 °C
44.3 ft-lb

@Temperature 73.4 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..
Dart Drop, Total Energy 60.0 J

@Temperature -20.0 °C
44.3 ft-lb

@Temperature -4.00 °F
ASTM D3763
SABIC Innovative Plastics Xenoy® X4850 PBT+PC (Asia Pacific)
Xenoy X4850 is a hydrostable, high modulus, high ductile PC/PBT blend. Furthermore, this resin provides high chemicalresistance, very low creep, low CTE, excellent fatique and high heat dimensional ..