Polymer Property : Dart Drop, Total Energy = 12.2 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Dart Drop, Total Energy 6.19 - 12.2 J

@Temperature -20.0 - -20.0 °C
4.57 - 9.00 ft-lb

@Temperature -4.00 - -4.00 °F
Average value: 9.19 J Grade Count:1
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..
Dart Drop, Total Energy 6.19 - 12.2 J

@Thickness 3.18 - 3.18 mm
4.57 - 9.00 ft-lb

@Thickness 0.125 - 0.125 in
Average value: 9.19 J Grade Count:1
Overview of materials for Nylon 66, 30% Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Carbon Fiber Filled". Specific grades with carbon fiber content between 25% and 34% are in..