Mechanical Properties Metric English Comments
Dart Drop, Total Energy 2.00 J

@Temperature -20.0 °C
1.48 ft-lb

@Temperature -4.00 °F
ASTM D1709-85
Mapal Plastics Maplon Type H Polypropylene Sheet
Properties : Good resistance to low temperatures, Moderate stress whitening, Suitable for die cutting, Corona treated on both sides for offset and screen printing.Applications : Stationery, Printing..
Dart Drop, Total Energy 2.00 J

@Temperature -30.0 °C
1.48 ft-lb

@Temperature -22.0 °F
Instrumented Impact Energy @ peak, -30°C @ 6.6 m/s; ASTM D3763
SABIC Innovative Plastics SABIC PPCOMPOUND 7985 PP
SABIC® PPcompound 7985 is a mineral filled, impact modified polypropylene TPO. This material combines scratch resistance and heat stability with interior automotive UV stability. The IMDS is 2097..