Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Hardness, H358/30 | 132 MPa | 19100 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 412 PBT (Europe-Africa-Middle East) VALOX 412 is 20% glass reinforced PBT injection moulding resin. Applications: Spotlights, appliance housings and handles. |
|||
Hardness, H358/30 | 132 MPa | 19100 psi | ISO 2039-1 |
SABIC Innovative Plastics Valox® 553 PBT (Europe-Africa-Middle East) VALOX 553 is a 30% glass fibre reinforced, flame retardant PBT+PC blend with good warpage characteristics. Applications: appliance handles, spotlights, electric motors, pumphousings. |