Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.0175 GPa | 2.54 ksi | ISO 37 |
Lubrizol ESTANE® 58144 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
50% Modulus | 0.0175 GPa | 2.54 ksi | DIN 53504 |
Lubrizol ESTANE® ETE60DT3 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |