Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.000800 - 0.00150 GPa | 0.116 - 0.218 ksi | DIN 53504 S2 |
Wacker Silicones Geniomer® 140 Silicone TPE SLM TPSE 140 is a silicone copolymer containing over 90% siloxane. Geniomer® is a two phase block copolymer made up of a soft polydimethylsiloxane (PDSM) phase and a hard aliphatic isocyanate phas.. |