Mechanical Properties | Metric | English | Comments |
---|---|---|---|
50% Modulus | 0.0180 GPa | 2.61 ksi | ISO 37 |
Lubrizol ESTANE® GP60DE Ester Based Thermoplastic Polyurethane Estane® GP 60DE is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding partsAvailable in EuropeInformation provided by Lubr.. |