Polymer Property : Tensile Creep Modulus, 1000 hours = 450 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 450 - 980 MPa
65300 - 142000 psi
Average value: 706 MPa Grade Count:14
Overview of materials for Nylon 66, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr..
Tensile Creep Modulus, 1000 hours <= 450 MPa
<= 65300 psi
DIN 53444
Zell-Metall Engineering Plastics Zellamid 1100 OIL at 50% RH
Zellamid® 1100 OIL: A new type of cast nylon produced by addition of a special oil to the polymer structure. By laboratory test it was proven that this second generation oil filled product reduces ..
Tensile Creep Modulus, 1000 hours <= 450 MPa
<= 65300 psi
DIN 53444
Zell-Metall Engineering Plastics Zellamid 1115 at 50% RH
By special additives, impact strength and abrasion resistance are further improved. We particularly recommend this material for slipper pads for rolling mills.Color: IvoryApplications: slipper pads ..