Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Creep Modulus, 1000 hours | 2900 MPa | 421000 psi | At 1% Deformation; DIN 53444 |
Wolf Kunststoff ZEDEX® ZX-100MT A1T Polymer Alloy, Mineral Reinforced Stiff; Hard; Very high strength; No fiber reinforcementApplications: Handling, Vessel and Pump, Steel and Water, Chemical Engineering, Automotive Technology, Machine ToolsInformation provided by Zed.. |
|||
Tensile Creep Modulus, 1000 hours | 2900 MPa | 421000 psi | ISO 899-1 |
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityEasy rel.. |
|||
Tensile Creep Modulus, 1000 hours | 2900 MPa | 421000 psi | ISO 899-1 |
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled ISO 7391-PC,MFLR,(,,)-09-9,GF10Global gradeMVR (300 °C/1.2 kg) 6.0 cm3/10 min10 % Glass fiber reinforcedChlorine- and bromine-free flame retardantUL 94V-0/1.5 mm and 5VA/3.0 mmHigh viscosityUV stab.. |