Polymer Property : Tensile Creep Modulus, 1000 hours = 1400 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Creep Modulus, 1000 hours 1400 MPa
203000 psi
Polycasa Acryl® G 88 Acrylic
Glazing, domed roof lights, lighting covers, publicity lighting, reflectors, lenses, instrument covers, dishes and bowls; mostly used in the automotive industry.Data was collected by ISO methods.Qui..
Tensile Creep Modulus, 1000 hours 1400 MPa
203000 psi
ISO 899-1
Lanxess Pocan® B 1300 000000 PBT
PBT, non-reinforced, injection molding, extrusion
Tensile Creep Modulus, 1000 hours 1400 MPa
203000 psi
ISO 899-1
Lanxess Pocan® B 1305 000000 PBT
PBT, non-reinforced, injection molding
Tensile Creep Modulus, 1000 hours 1400 MPa
203000 psi
ISO 899-1
Lanxess Pocan® KU 1-7301 000000 PBT
PBT, non-reinforced, injection molding, food contact
Tensile Creep Modulus, 1000 hours 1400 MPa
203000 psi
ISO 899-1
Lanxess Pocan® KU 2-7003 000000 PBT
PBT, non-reinforced, injection molding
Tensile Creep Modulus, 1000 hours 1400 MPa
203000 psi
ISO 899-1
Lanxess Pocan® KU 2-7503/1 000000 PBT
PBT, non-reinforced, injection molding, extrusion, flame retardant
Tensile Creep Modulus, 1000 hours 1400 MPa

@Strain <=0.500 %
203000 psi

@Strain <=0.500 %
ISO 899-1
Styrolution Luran® S 757 R Colored ASA
Description: General-purpose grade for injection molding with high stiffness.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Tensile Creep Modulus, 1000 hours 1400 MPa
203000 psi
ISO 899
Styrolution Luran® S 767KE ASA
Luran S 767KE is particular suitable for co-extrusion with PVC at low temperature. Hereby, it provides a glossy surface finish.Enhanced flowabilitySuitable for co-extrusion with PVCEnables high glos..
Tensile Creep Modulus, 1000 hours 1400 MPa
203000 psi
ISO 899
Styrolution Luran® S 777 K ASA
Luran S 777 K is an easy flowing injection molding ASA grade with good toughness and heat distorsion resistance.
Tensile Creep Modulus, 1000 hours 1400 MPa

@Strain <=0.500 %
203000 psi

@Strain <=0.500 %
ISO 899-1
Styrolution Luran® S 777 K UV Black 56625 ASA
Description: Easy flowing injection molding grade with good toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS
Tensile Creep Modulus, 1000 hours 1400 MPa
203000 psi
ISO 899
BASF Ultraform N 2320 003 UNC Q600 POM
Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent.
Tensile Creep Modulus, 1000 hours 1400 MPa
203000 psi
ISO 899
BASF Ultraform N 2320 U03 UNC Q600 POM
Ultraform N2320 U03 UNC Q600 is a rapidly freezing UV stabilized general-purpose injection molding grade.
Tensile Creep Modulus, 1000 hours 1400 MPa

@Strain <=0.500 %
203000 psi

@Strain <=0.500 %
ISO 899-1
BASF Ultraform® N2770 K POM
Description: Is a POM, injection-molding grade with improved wear characteristics for sliding elements.Information provided by BASF
Tensile Creep Modulus, 1000 hours 1400 MPa
203000 psi
Arkema Group Oroglas® VS-UVT Acrylic, Injection Molding Grade  (discontinued **)
The outstanding flow of OROGLAS VS-UVT makes it as the material of choice for injection molding of part with thin wall thickness.The ultraviolet transmitting ( uvt) formulation is developed to meet ..
Copyright © lookpolymers.com All Rights Reserved