Polymer Property : Heat Seal Strength Initiation Temperature = 80.0 °C Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 80.0 °C
176 °F
ASTM F88
NatureWorks® Ingeo™ 4060D Sealant Grade PLA
PLA (polylactide) polymer 4060D can be coextruded with other PLA resin to form a sealant layer for biaxially oriented PLA film. This resin has excellent heat seal and hot tack performance with a sea..