Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength Initiation Temperature | 135 - 191 °C | 275 - 375 °F | 1 sec @40 psi |
DuPont Teijin Films Melinex® 3381 Polyester Film Melinex® 3381 is a two-side heat sealable, opaque white polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well a.. |
|||
Heat Seal Strength Initiation Temperature | 135 - 191 °C | 275 - 375 °F | 1 sec @40 psi |
DuPont Teijin Films Melinex® 342 Polyester Film Melinex® 342 is a two-side heat-sealable, clear polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well as a vari.. |
|||
Heat Seal Strength Initiation Temperature | 135 - 191 °C | 275 - 375 °F | 1 sec @40 psi |
DuPont Teijin Films Melinex® 357 Polyester Film Melinex® 357 is a two-sided heat sealable, opaque white polyester film which is ideal in specialty card laminate applications. This film can be heat sealed to itself and other polyesters, as well a.. |