Polymer Property : Heat Seal Strength Initiation Temperature = 230 °F Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Heat Seal Strength Initiation Temperature 110 °C
230 °F
1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7028 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin General Purpose Resin Excellent Strength Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a (with Restrictions) TUFLIN™ HS-7028 NT 7 is an ethylene-hexene copolymer, de..
Heat Seal Strength Initiation Temperature 110 °C
230 °F
1 lb/in heat seal strength; 0.5 sec dwell, 40 psi bar pressure, pull speed 10 (in./min.); Dow Method
Dow TUFLIN™ HS-7046 NT 7 Linear Low Density Polyethylene Resin
Hexene Linear Low Density Resin Slot Cast Extrusion Outstanding Drawdown Capability Complies with U.S. FDA 21 CFR 177.1520 (c) 3.1a TUFLIN™ HS-7046 NT 7 is an ethylene-hexene copolymer, designed f..
Heat Seal Strength Initiation Temperature 110 °C
230 °F
Braskem Method
Braskem RP 344 RACO Random Polypropylene Copolymer
RP 344 is a medium melt flow rate random copolymer. It is suitable for blown and cast film extrusion and features good processability, excellent optical properties, and outstanding sealability. Its ..