Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Heat Seal Strength Initiation Temperature | 125 °C | 257 °F | Average value: 125 °C Grade Count:6 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Heat Seal Strength Initiation Temperature | 125 °C | 257 °F | Sealing Initial Temperature; Braskem® Method |
Braskem ES 300 HDPE Blown Film Extrusion Polyethylene
(discontinued **) 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags; high-strength films. Informa.. |
|||
Heat Seal Strength Initiation Temperature | 125 °C | 257 °F | |
Hyosung Topilene C600HF PP C600HF Film Grade Butane Random CopolymerApplications: Sealable CPP/OPPCharacteristics:Low sealSlip propertyTransparencyInformation provided by Hyosung Corporation |
|||
Heat Seal Strength Initiation Temperature | 125 °C | 257 °F | Braskem Method |
Braskem GM9450F HDPE Blown Film Extrusion Polyethylene HDPE GM9450F is a high-density polyethylene developed for the high molecular weight film extrusion segment produced with bimodal technology. The film produced from this resin has high tenacity and e.. |
|||
Heat Seal Strength Initiation Temperature | 125 °C | 257 °F | |
Braskem Green PE SGM9450F Blow Film Extrusion and Cast Film Extrusion High Density Polyethylene Description: SGM9450F is a high-density polyethylene, developed for the high molecular weight film extrusion segment produced with bimodal technology. The film produced from this resin has high tena.. |
|||
Heat Seal Strength Initiation Temperature | 125 °C | 257 °F | Sealing Initial Temperature; Braskem® Method |
Braskem HF 0150 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |
|||
Heat Seal Strength Initiation Temperature | 125 °C | 257 °F | Sealing Initial Temperature; Braskem® Method |
Braskem HF 0144 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |
|||
Heat Seal Strength Initiation Temperature | 125 °C | 257 °F | Sealing Initial Temperature; Braskem® Method |
Braskem HF 0147 HDPE Blown Film Extrusion Polyethylene 38µm film gauge, obtained in 75mm extruder, die gap 1.0mm, output 1.75 kg/h-cm with 2:1 BUR. Applications: Grocery and T-shirt bags; merchandise bags; frozen-food bags. Information provided by Bras.. |